We recently received some raw boards from a vendor and we typically do an
inspection sample when they are received. It was not noticed during the
sample but was found later that there were some very small areas located on
traces that the masking had flaked off. Is it a possibility just for my own
satisfaction that the masking could of flaked off during the manufacturing
process. We do a tape test on 1 piece when the boards arrive also both on
masking and on gold contacts.
Does the color of masking make a difference? These were masked in Black!
Any comments?
Gloria
phone 906-932-5970 ext. 26
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------