Hi Wayne,
apologies to you and the rest of the forum for not clarifying, the mark you
can see is a probe mark from the supplier testing (separate issue), this was
the best picture I could get in the time available.
regards,
Pat
-----Original Message-----
From: Wayne Thayer [mailto:[log in to unmask]]
Sent: Monday, November 27, 2006 5:57 PM
To: [log in to unmask]
Subject: Re: [TN] Soldering Anomaly
Pat-
What the devil is that thing in the very center of the photograph? Is
it a projection? Looks like it projects out and leans to the
right--kind of looks like a silver pony tail, and it looks like the
solder is backed off from it.
Please clarify.
Wayne Thayer
>>> [log in to unmask] 11/27/2006 12:23 pm >>>
Hi Everyone!
Well, I finally got Pat's picture up! The reason it's taken me so long
is
because I'm back home in North Carolina, and the only internet access I
have
is dial-up at a screaming 26.4 KB per second! I remember not that long
ago
that was fast. But once you get used to a DSL or T1 connection, well
that's
just dog slow.
Anyways, here's Pat's picture:
http://www.stevezeva.homestead.com/files/solder_anomaly2.JPG
To me that doesn't look right. I've soldered with a Sn62/Pb36/Ag2
paste
before and soldered lead-free components on a ENIG board and the
joints
didn't look that rough. That's more than just cooling lines IMHO...
-Steve Gregory-
----- Original Message -----
From: "Diamond, Pat" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, November 27, 2006 2:12 AM
Subject: [TN] Soldering Anomaly
> Hi Technetters,
>
> We have recently received some assembled boards from a new supplier
and
> upon
> carrying out a First Article Inspection on them I noticed what I
thought
> were disturbed solder joints. I then referred to IPC-610 which
seemed to
> confirm this. Upon talking to the supplier about this problem they
said
> that this was not disturbance but "cooling lines" due to the fact
that the
> component leads were lead-free and the solder paste was
Sn62/Pb36/Ag2.
> They referred me to IPC-610 Para. 5.2.7 Fig. 5.56 (page 5-18) which
looks
> nothing like the joints on our components. The only area this
anomaly is
> occurring is on the SOT 23 Transistors & Diodes.
> Our company is not a main line SMT producer and I have never seen
this
> anomaly before.
>
> I have contacted Steve Gregory and he has kindly agreed to post a
couple
> of pictures on his website for me, see what you think.
>
> I really hope they are cooling lines!!!
>
> Thanks in advance for any help/advice you can offer.
>
> Best regards,
>
> Pat
>
>
>
****************************************************************************
> ***************
> The information transmitted is intended only for the person or entity
to
> which it is addressed and may contain confidential and/or privileged
> material.
>
> Any review, retransmission, dissemination or other use of, or taking
of
> any
> action in reliance upon, this information by persons or entities
other
> than
> the intended recipient is prohibited. If you received this in error,
> please
> contact the sender and delete the material from any computer.
>
****************************************************************************
> ***************
> Mr Pat Diamond
> Senior Specialist Engineer
> Weston Aerospace Tel: +44 (0)1252 868122
> 124 Victoria Road Fax: +44 (0)1252 370298
> Farnborough, Hampshire, GU14 7PW Web www.westonaero.com>
> England Email mailto:[log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
[log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|