TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Date:
Mon, 6 Nov 2006 08:31:25 -0500
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
R&D Assembly
MIME-Version:
1.0
Parts/Attachments:
text/plain (111 lines)
About a year ago we did some "rule of thumb" thinking on this subject. You
might check the archives.
I think we came up with a number like 15 micro inches with a 5 mil stencil.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Monday, November 06, 2006 8:14 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement

        Inge:
              15 micrometers thickness is almost 600 mils. About 6 times the
"safe" thickness allowed by J-std-001. Have you seen gold embrittlement with
less than 100 mils, or anyone else? It would be interesting to know.
Comment, there is a lot of waste of gold by electroplating instead of using
Immersion.
        Regards,
        Ramon

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Monday, November 06, 2006 4:00 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement

Agree,
We degold all microwave SMT small outline transistors ("helicopters"),
because we had catastrophic gold embrittlement problems. The solder joints
were so brittle, that the leads lifted from the pad in the temp cycle tests.
We measured as much as 15 micrometers of gold! The semiconductor
manufacturer meant, that it is a problem to have control on the gold process
on such small parts. What nonsense! Anyway, we are today suspiscious with
many gold plated parts and do degolding rather than getting embrittlement.

I'll send some pictures to Steve, so you can see what can happen.
Horror!


Inge


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: den 2 november 2006 23:06
To: [log in to unmask]
Subject: Re: [TN] Gold Embrittlement

Hi Amol,
I you have imersion Au, Au-embrittlement is not a problem because there is
not enough Au. Be careful, however, if your PCBs come from China; I have
seen much thicker Au-layers than are possible with iAu.
Calculating the wt% of Au in a soldert joint is an exercise in futility,
because you have to make the assumption--frequently not warranted--that the
SnAu-IMCs are uniformally distributed.
In cases where you suspect thicker Au [and for the matter Ag; which is
equally as bad as Au in causing SJ-embrittlement] deposits, the safest
course of action is to wash the Au (Ag) off by tipping.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2