There are changes to those two slash sheets that will be reflected in
Supplement 1, but right now those values are the following:
* /126 Tg is 170 degrees C minimum
* /129 Tg is 170 degrees C minimum
* /126 Td is 340 degrees C minimum
* /129 Td is 340 degrees C minimum
* /126 T260 is 30 minutes minimum
* /129 T260 is 30 minutes minimum
For the lack of a better definition, these two slash sheets are mine. If
you want to know more about the Dewey diligence that went into these,
give me a call.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Geoff Layhe of Lamar
Group
Sent: Thursday, November 30, 2006 6:49 AM
To: [log in to unmask]
Subject: [TN] IPC4101B/126 7 129
I haven't received my copy of 4101B yet so can someone tell me what /126
and /129 are
Tg, Td, T260 etc,
many thanks
Geoff Layhe
Private & Confidential:
This e-mail message is confidential and is intended solely for the
person or organisation to whom it is addressed. If the message is
received by anyone other than the addressee please return the message to
the sender by replying to it and then delete the message from your
computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|