How many layers is that? It looks like a 4 layer with delam in the core.
Geoff Layhe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of stephen gregory
Sent: Wednesday, November 29, 2006 5:12 PM
To: [log in to unmask]
Subject: Re: [TN] FW: Delamination pics (IS410)
Good Morning to you Gloria!
I've got your Word doc. file with the pictures posted at:
http://www.stevezeva.homestead.com/files/dELAM.doc
Looking at the pictures, I'm assuming that each page shows images from a different area. It's worth noting that the delamination appears to be at the same layer, or am I wrong about that?
What is your fab vendor saying about this problem?
What I'm about to say isn't trying to slam all board houses, but in all the years that I've been working in this business, I've found that almost never will a board house fairly compensate a company after they've found a problem with a fab after it's been built. Most of the time they've said they will give us new boards, but won't compensate us for the labor and materials in the assembly, and I think that sucks.
Looking at all the pictures you've sent us, I definitely think it's a fab problem, not any of your assembly processes, and I would be leery of shipping any product that is using these fabs.
But that's just my opinion...
-Steve Gregory-
Gloria Brown <[log in to unmask]> wrote:
Good Morning Steve,
We had a micro section completed on the delaminating area of the boards here that we are finding that same issue with. Thought I would share them as well. I know that I cannot send them to the forum so if you can post them like you did the others and share them also please do.
Thanks
Gloria Brown
phone 906-932-5970 ext. 26
fax 906-932-9822
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Private & Confidential:
This e-mail message is confidential and is intended solely for the person or organisation to whom it is addressed. If the message is received by anyone other than the addressee please return the message to the sender by replying to it and then delete the message from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|