Hi Pearl
As any delamination may be in a localized small area, it may be missed
when trying to do a series of hand soldering tests. You may be
interested in the method that I have adopted to check full panels that
involves passing them through a reflow oven having a temperature profile
that provides a thermal shock of sorts. The settings that work for me
provide a temperature gradient of 80 degrees C per minute to reach a
maximum temperature of 290 degrees in just under 4 minutes with a
similar cooling curve. I find that good boards will survive a double
pass and defective boards will fail on one pass. It also gives you a
good idea of how good your immersion silver finish is ~ a good finish
will dull down slightly after one pass and become slightly
tarnished/yellow after 2 passes.
Regards
Alistair Murray
Artetch Circuits Ltd
England UK
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of pearl petras
Sent: 28 November 2006 16:59
To: [log in to unmask]
Subject: Re: [TN] More delam
This is standard FR4 with immersion silver finish.
The standard soldermask colour we spec is clear, not green. Allows us
to better see the copper, and often some inner layer features as well,
but if you aren't used to working with FR4 with clear soldermask, it can
definitely look a little strange, at first.
The dark colour seen is due to an inner layer that is primarily ground
plane.
I'm pretty sure that it isn't soldermask bubbling
We have not yet done any microsectioning. So far we have only seen
this on fully populated boards that have experienced some
hand-soldering, and we are reluctant to sacrifice one, if it can be
saved for production.
I have a blank two-up panel available from each manufacturer we've
used. We are planning to run some hand-soldering tests. Vary
temperatures, one unbaked and one baked from each panel, etc. Any other
ideas?
---------------------------------
All new Yahoo! Mail -
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
Get a sneak peak at messages with a handy reading pane.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|