TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Fri, 17 Nov 2006 15:29:20 -0500
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
R&D Assembly
MIME-Version:
1.0
Parts/Attachments:
text/plain (83 lines)
Actually, neither IPC standard requires rework or repair. They require
disposition. Disposition may include rework, repair, use "as is", re-grade .
. . These come to mind.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Friday, November 17, 2006 10:17 AM
To: [log in to unmask]
Subject: Re: [TN] One solder Ball Not Connected on a No Connect Pad After
Rework

When the pad is lifted, it typically exposes the fiberglass weave underneath
the pad. This allows moisture, flux, solvents, etc,  to enter the pwb and
can cause problems later.
The answer to your question depends on what the assembly is used for, and to
what standard do you wish to comply with. IPC 610 and J-STD-001 do not allow
missing pads, they require it be repaired.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of bob wettermann
Sent: Friday, November 17, 2006 9:11 AM
To: [log in to unmask]
Subject: [TN] One solder Ball Not Connected on a No Connect Pad After Rework

This question to the group is about expected solder joint strength on a BGA.

  The BGA in question is a 8 x 8mm plastic package  BGA using a LF
SAC305 soldering process. It has 64  x 0.018" balls holding it to  the PCB.

  When removing this device for rework 3-4% of the time one of the corner NO
CONNECT pads comes off.

  The question is if we do nothing upon replacement of  a new device  to the
damaged pad will it really make a difference ??? We are arguing that the
holding strength of the reworked device would be approximately the same
because the change in overall surface area is marginally impacted.


  Thanks

  Bob Wettermann


Bob Wettermann

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
PH 847-767-5745

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2