Hi 'JaMi,'
While I agree with you about the appearance of these solder joints, I cannot
agree with you regarding what would happen in the absence of Au.
If you make the leads and their attachment area larger [which from electrical
and thermal conductivity considerations is advantageous], you run into
another problem.
For this type of devices, the lead material is typically Alloy 42, not Cu.
Thus, large soldered areas will suffer from local expansion mismatches in
combination with the global expansion mismatches.
In any case, the excessive amount of Au does not help.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|