Mornin' Les!
Gracious no! None of our military customers are lead-free...
-Steve-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - Bogert
Sent: Wednesday, November 01, 2006 5:35 PM
To: [log in to unmask]
Subject: Re: [TN] Bizzare Phenomena...
November 1, 2006
I can offer no help Steve, but can you tell me if your lead-free
customers are military equipment?
----- Original Message -----
From: Steve Gregory<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Tuesday, October 31, 2006 9:57 AM
Subject: [TN] Bizzare Phenomena...
Mornin' All!
This morning I have seen something that I have never, ever have seen
before. It's been a little slow the past week, so we decided to do our
maintenance on our reflow ovens. After we opened the oven up, we found
many, many solderballs laying on the bottom of the oven right around
zone 7 - 8, right at the beginning of the spike zone. Check-out:
http://stevezeva.homestead.com/files/Oven_Solderballs.jpg<http://steveze
va.homestead.com/files/Oven_Solderballs.jpg>
http://stevezeva.homestead.com/files/Oven_Solderballs_2.jpg<http://steve
zeva.homestead.com/files/Oven_Solderballs_2.jpg>
http://stevezeva.homestead.com/files/Oven_Solderballs_3.jpg<http://steve
zeva.homestead.com/files/Oven_Solderballs_3.jpg>
http://stevezeva.homestead.com/files/Oven_Solderballs_4.jpg<http://steve
zeva.homestead.com/files/Oven_Solderballs_4.jpg>
We've been having tombstoning problems when we've run the two
lead-free
jobs that we have here. I've been working with the paste vendor
sending
my profiles and plots, but I haven't been able to solve the problem.
The
solderballs in the oven are lead-free solderballs.
We are using a Heller 1809, and my profile set-points are:
120 140 160 180 190 200 230 240 250
120 140 160 180 190 200 230 240 250
Belt speed 26 in per min
The paste is a SAC 305 with a water washable no-clean flux. I think my
profile is pretty reasonable, and the last board we ran is pretty
standard, .062" thick, with no bizzare copper planes. The board finish
with both jobs has been ENIG. The last job I ran we were tombstoning
0805's, the one before that we were tombstoning 0402's. With both jobs
we've had major tombstoning problems. I've slowed the beltspeed down,
sped it up, ramped up slower, ramped up faster, changed this, changed
that, but still haven't resolved my tombstoning.
Of course, I'm the only one that's having this problem according to my
paste vendor...
I wouldn't have imagined that I would see the solderballs in the oven
like we have...
Have any of you ever seen something like this before?
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont
entpage.asp?Pageid=4.3.16> for additional information, or contact Keach
Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|