DESIGNERCOUNCIL Archives

September 2006

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
DesignerCouncil <[log in to unmask]>
X-To:
Designers Council Forum <[log in to unmask]>
Date:
Wed, 6 Sep 2006 10:07:31 +0100
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, Matthew Lamkin <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Matthew Lamkin <[log in to unmask]>
Parts/Attachments:
text/plain (58 lines)
Simple, when they are putting the solder mask screen over the top of the board to screen it, they need a certain amount of play, as it may not always be placed 100% in the exact location.

I.E. if it was 1:1 there is a chance that a slight misalignment can cause solder mask to be put on the pads.

It is usual for solder mask to be 8 thou bigger than the pads, as for standards I have no idea, it's the manufacturers that insist on this, if we do not provide a soldermask that is bigger, then they will simply increase it to suit.

For fine pitch IC's etc it is common to have a block of mask missing rather than individual pads as it is very hard to put it accurately on fine pitched pads, the tolerances won't match.

Although, this has the effect of sometimes allowing more solder shorts so the design has to be done to take this into account, as are the assembly depts required to be informed to watch for it.

Matthew.

-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]]On Behalf Of No
Name
Sent: Wednesday, September 06, 2006 7:00 AM
To: [log in to unmask]
Subject: [DC] Soldermask - question?


   Hi All,

 I am recently shifted into PCB design filed; interesting field off course!!! satisfied being a part of product development.
 Now started learning the reason for each task I perform. Hope I can get more suggestions from expertise here :-).

 I understand the reason that slodermask is used for better solderability, but I want to know why we provide certain clearance like 0.005" or 0.004" more than pad size, sometimes I see soldermask missing (say on BGA). Any problems you have experienced due to larger or smaller soldermasks?

 Is there any specific standards or calculation used for soldermask creation based of padstack,Assembly process say wave soldering or reflow soldering? How IPC calculates this? I have IPC SM782.

 Awaiting for your suggestions.

 Thanks,
 Raja.


    Check out AOL.com today. Breaking news, video search, pictures, email and IM. All on demand. Always Free.

________________________________________________________________________
Check out AOL.com today. Breaking news, video search, pictures, email and IM. All on demand. Always Free.

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2