TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 9 Aug 2006 12:09:54 -0700
Reply-To:
Subject:
From:
Miguel Vallejo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
Organization:
Altatron EMS
MIME-Version:
1.0
Parts/Attachments:
text/plain (44 lines)
Hi guys,

Can any one share your experience with the increase amount of dross
production from your lead-free wave operation?

I'm using SN100C alloy on an air atmosphere. I'm seeing 84% of the solder
used turning to dross (6.2:1 efficiency ratio).

In my study, I weighted the loaded board prior to and after wave solder to
determine the amount of solder on each PCBA, and compared the amount of
solder used to replenish the pot with the aggregate amount of solder
required on 15K units. The difference correlates with the amount of dross
produced.



I'd like to understand how much of this increase is attributed to the
lead-free technology and how much to the equipment performance.



Thanks for your help.



Miguel Vallejo

Mfr Engineer






---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2