There is a reference on the site by the work done in Switzerland; it can be
downloaded from this page:
http://www.rohsusa.com/page20.html
Download the report on tin whiskering at the bottom of the page.
John
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of MA/NY DDave
Sent: Monday, May 22, 2006 8:35 PM
To: [log in to unmask]
Subject: Re: [LF] Back to square one
Hi J-P, Joe, Werner, ALL, IPC LF Listservers,
I have to read all your notes, yet in support of LF failures Tin Whiskers
has been reported as a real failure mechanism that is unique to Pb-free.
By that I mean we have more than just accelerated failures or modelling
failures.
One published failure is in space via NASA and another, I and we know of,
is in a Nuclear Reactor facility in CT. I called them once or twice, yet
still have to do some more follow up. If anyone else has done this please
Share.
We also should expect SnCu failures with P-I-Hole components, as well as
some chip capacitor end cap failures.
I do agree that hard published data is going to take some time to work
it's way to the public domain so that everyone will have some references.
Yours in Engineering, Dave
YiEngr, MA/NY DDave
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|