TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Tue, 30 May 2006 17:43:40 -0400
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=us-ascii
Subject:
From:
Andrew Shieh <[log in to unmask]>
Parts/Attachments:
text/plain (93 lines)
John, et. al.

Thanks for the various suggestions.  We have had some experience with "3D
XRay"
systems in the past and will try it out on our solder ball joints.  I will
share the results
with the net if we learn anything noteworthy.

Andy






John Burke <[log in to unmask]> on 05/30/2006 12:59:56 PM

Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to
      John Burke <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: Andrew Shieh/CSP)
Subject:  Re: [TN] solder ball analysis




I used that type of system and it will definitely find the issues,
particulary useful on a co-planar defect at the boards interface.

I used this system 2 years ago up north of San Francisco I think, it cost
about $4000 for the set up plus about the same for the shots, but the
results were incredible, you can literally "fly" through the 3D Xray using
the software.

If needed I wil dig up th company and details of the people and send off
line.

John

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Tuesday, May 30, 2006 8:29 AM
To: [log in to unmask]
Subject: Re: [TN] solder ball analysis

When you are looking at the balls on the BGA for this analysis, what
features are you looking to find?  Crack? Opens? Unsoldered balls?  I  know
that
Micro-CT imaging can get down to sub-micron feature sizes in  3-D.  Does
that get
you the detail you need?

Jon Moore

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2