Phil.... you are of course correct that Gold does not tarnish... however, the Nickel does, and the Gold may be (read as "almost certainly is") porous....
I have to believe that re-sealing the boards in an airtight package SHOULD be adequate protection, but then this might not give the vendor a way to get off the hook
;-)
Rudy Sedlak
RD Chemical Company
Phil Nutting <[log in to unmask]> wrote:
Good Friday Morning All,
This topic may have been previously discussed, but let me try to phrase
my "problem" completely so the answer can be simpler.
I have a board vendor (Fab house) stating that for my ENIG boards the
plating only has a 6 month shelf life if the package is opened. Did I
miss something here? I thought Gold doesn't tarnish.
If this is true, then Immersion Tin, Immersion Silver and ENIG all have
storage issues.
OK, so I open a sealed package and take out half of the boards in the
package. I may not need the rest of the boards for many months. So how
do I protect the unused boards? Should I vacuum seal them? Add a
desiccant? If I add a desiccant, are there different desiccants which
might damage the boards?
I'm sure I'll have more questions right after I send this.
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Love cheap thrills? Enjoy PC-to-Phone calls to 30+ countries for just 2¢/min with Yahoo! Messenger with Voice.
|
|
|