TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Lin Leo <[log in to unmask]>
Date:
Tue, 25 Apr 2006 10:47:17 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (47 lines)
Leo:

You are having this problem on both HASL and immersion Tin boards?
This would imply that the cause of the problem is before either is applied.

What are you using for an etch resist?  Tin or Tin Lead, or photoresist?

Rudy Sedlak
RD Chemical Company

Lin Leo <[log in to unmask]> wrote: Hi,

       I met ionic contamination problem at HASL and Immersion Tin surface finish board.(SEC values were measured from instrument Omega 600)  I found significant difference at different patteren.  The more through holes, the higher ionic contamination.

       Did anyone experience in this phenomena?  Any literature/report has discussed the factors resulted in the ionic contamination?  How to clean the boards to decrease this defect?

  Thanks

  Leo


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
___________________________________________________  最新版 Yahoo!奇摩即時通訊 7.0,免費網路電話任你打!  http://messenger.yahoo.com.tw/



---------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
New Yahoo! Messenger with Voice. Call regular phones from your PC and save big.

ATOM RSS1 RSS2