I guess I got this thru technet somehow. As long as I did let me ask
...You wouldn't know anything about solder mask problems would you? We
have a weird one that dupont (vacrel 8140) and our pc bd mfr say they've
never seen. It a chipping or lifting (hard to tell which) of solder mask
around the annular rings and along short pieces of copper traces. It
passes the pencil test and peel however. It looks like whatever happened
was an event that hasn't gotten worse - but the bds are basically
useless now.
p
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Thursday, March 23, 2006 10:59 AM
To: [log in to unmask]
Subject: Re: [TN] Die Punching PWBs as opposed to drilling and NC
routing
Thanks for the insight George.
I was curious about the maximum number of holes punched at one time but
worded that part of my query poorly.
Very best,
Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|