Frank
If you follow this route be careful that you check each material component. I recently found a soldermask that was in use that contained lead. On the other hand if you are going to verify the compliance after the board is fabricated about the only analytical tool available is Auger.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: Franklin Asbell<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Monday, December 19, 2005 9:33 AM
Subject: Re: [TN] verifying RoHS Compliance
XRF won't provide you percentage of alloys unless specific calibrations are
programmed into it.
I'm curious, wouldn't the certificate of analysis of the raw material be
sufficient for verifying compliance? The raw material supplier is performing
the test, why would it need repeating?
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Monday, December 19, 2005 8:24 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] verifying RoHS Compliance
Trevor,
I will not ask where this information is, I have not studied the directives.
But it would be good to know the source, though ;o)
What I wonder is how will it be measured? In the assembler's incoming it
would be OK to scrape the plating off and put the part on the XRF, but once
we deal with finished product, it gets rather complicated.
Thanks,
Ioan
> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Trevor Chainey
> Sent: Monday, December 19, 2005 9:06 AM
> To: [log in to unmask]<mailto:[log in to unmask]>
> Subject: Re: [TN] verifying RoHS Compliance
>
> Phil/Mike,
>
> Lead up to a maximum of 4.0% is permitted in copper alloy.
>
>
> Trevor Chainey
> Quality Manager
> Telesoft Technologies Ltd
> Telephone +44 (0)1258 486568
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|