Its just a definition of which boards are defective within a panel. We
simply had the board vendor X them out and place a round tape dot over
the fiducials so the pick and place machine skips that board on the
panel.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin Asbell
Sent: Wednesday, November 16, 2005 7:54 AM
To: [log in to unmask]
Subject: Re: [TN] X-Outs
You need to define it for coworkers?
As far as I know there is not "official" explanation or definition for
"X-Outs".
It is performed to achieve one or more of the following;
A defective board within an array will be identified to ensure it is not
used (populated, further processed, etc). Typical methods of "X-Out"
include an "X", obviously, in indelible ink. Marking with etching pen,
razor knive, etc. or other means to ensure the product is clearly
identified as unsuitable for use.
In the past the board was just punched or drilled to signify unfit for
use.
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken
Sent: Tuesday, November 15, 2005 7:21 PM
To: [log in to unmask]
Subject: [TN] X-Outs
Hi all,
Does the IPC or anyone define the term "X-Out" officially?
I've used the term for years at other companies but now need to define
it for my current co-workers.
Thanks.
Ken
------------------------------------------------------------------------
----
---
Kenneth J. Wood C.I.D
Saturn PCB Design
2737 Bishop Lane
Deltona, Fl 32725
407-340-2668
www.saturnpcb.com <http://www.saturnpcb.com/>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|