Eddie,
I think that there are books out that indicate the percentage of gold in
solder that will lead to brittle joints. I think the IPC spec says less than
0.2% gold in solder is acceptable. Your customer should be able to calculate
solder volume vs. Gold volume and determine the percentage. If it is below
the 0.2% he should be OK.
Joel Mearig
Delta Tau Data Systems, Inc.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eddie Rocha
Sent: Wednesday, October 26, 2005 10:50 AM
To: [log in to unmask]
Subject: [TN] ENIG and brittleness
I have a customer looking to convert over to ENIG but would
like to see information that shows he doesn't need to be
concerned with brittle solder joints. Where could I find
this type of information?
Thank you,
Eddie Rocha
South Bay Circuits
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|