Avionics uses many different solder for different application: some of them
required for field repair without cleaning. "do not use" may just apply to
one of the applications that can not use 331... unless you find out more
detail in the application notes or instruction (you might have to go all the
way back to the design files to find out the requirement), the best bet is
follow the instruction (use your spare time to find out why... it may take
longer than you thought... I ask someone went to a ware house to dig out 20
year old document before, just to varify a compatibility of a part that is
obsolete...).
my 1.72 cents.
jk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of prasad godavarti
Sent: Sunday, October 02, 2005 12:56 PM
To: [log in to unmask]
Subject: [TN] use fo high halide flux on avionics: kester 331 flux
does anyone have any information on the performance of
cored wire kester 331 fluxed sn-pb solder. I am
unable to find much in the literature, in fact all i
can see is words of caution: do not use. Thanks
__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
http://mail.yahoo.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|