Rich,
Per the ASM metals Handbook and UNS specification C26000, Pb is 0.07
Max.
Joseph
Joseph M. Oparowski
Center for Materials Science - Consulting and Failure Analysis
Bose Corporation [log in to unmask]
The Mountain, M/S 415 Phone: (508) 766-1371
Framingham, MA 01701-9168 Fax: (508) 766-1313
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Thursday, October 06, 2005 6:47 PM
To: [log in to unmask]
Subject: [LF] Brass CDA 260?
I have conflicting information on the max allowable % of lead in CDA 260
brass.
One reference claims a 0.07% max and the other claims 0.70%.
Does anyone know for sure?
Rich K / KEDS
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d To unsubscribe, send a message to [log in to unmask] with following
text in the BODY (NOT the subject field): SIGNOFF Leadfree To
temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL) Search previous postings at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|