Try IPC-4552
Dick Anderson
978-442-5165
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Adeline KO
Sent: Thursday, October 20, 2005 9:12 PM
To: [log in to unmask]
Subject: [LF] Brd finishing Immersion Gold with BGA. Had black spot
issue
Hi,
My process guy claim that immersion Gold brd with BGA will had black
spot
issue.
And my collegue claim that IPC has doc claim that this is not longer an
issue but she can't able to recall where she read this articule.
Any ppl happen to have this Doc and know where to find this doc.
Thks!
Rdgs
Adeline
Notice
The information in this message is confidential and may be legally
privileged. It is intended solely for the addressee. Access to this
message by anyone else is unauthorized. If you are not the intended
recipient, any disclosure, copying or distribution of the message, or
any action taken by you in reliance on it, is prohibited and may be
unlawful. If you have received this message in error, please delete it
and contact the sender immediately. Thank you.
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|