TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord <[log in to unmask]>
Date:
Wed, 19 Oct 2005 09:00:23 -0400
Reply-To:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<000001c5d488$170b3b60$9c7765d5@MONKEY>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (114 lines)
IngeMAR,
you just confirm what I have been observe many, many times... (1) complete
coverage (void free) and (2) soft (bond as soon as you get them) (3)batch to
batch consistancy...Otherwise, it is a killer... (good today, don't know
what going to happen tomorrow... like boy friend, girl friend thing...).
                                   jk

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord
Sent: Wednesday, October 19, 2005 4:36 AM
To: [log in to unmask]
Subject: [TN] SV: [TN] SV: wire bondable immersion gold


Joe,
Like many others, we have been experimenting with gold ball bonding on
nickel with a thin gold plate. With 6 sigma in mind, we were not
satisfied with the results. Reason seemed to be that there was a bad
match between the sof gold (HV~80) and the very surface of nickel
(HV~300). Tests on matte nickel performed well, but the board maker
could not plate matte nickel at that time. We tried doped gold wire with
various hardness, and got better results, but still not obtaining zero
bond failures we abandoned the project. Wedge gold wire bonding,
however, is different. We have made some products with this method on
0.05 um gold over nickel, and with good results.
Ingemar

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Joe Fjelstad
Skickat: den 18 oktober 2005 22:58
Till: [log in to unmask]
Ämne: Re: [TN] SV: wire bondable immersion gold

Hello Inge and Joyce,

You are right, Inge, that folks have been using very thin gold for
aluminum
wedge bonding for many years (and have even in some cases bonding
directly to
nickel as you mention).

The importance of thin gold with aluminum wire (and conversly thin
aluminum
with gold wire) is a hard won lesson left over from the days of the
"Purple
plague".

However, there actually is a link within the link that shows images of
ball
bonds not wedge bonds.

There is no process detail but the text reads (company name removed):

"Wire-bond process for high-temperature applications produces bonds that
are
stable at high temperatures with a thinner gold layer. These special
high-temperature wire bonds are especially useful in avionics and
automotive apps, and
require no additional lead time for production. The wire bond process
eliminates the Kirkendall voiding that takes place in an Al / Au
interface at 200°C
thermal exposures."

It is obvious from the wording that they have concerns of Kirkendall
voiding
and they are finding benefit in not making the bond directly to
aluminum. Even
so that is mighty thin gold for gold ball bonding to be sure. It is
impressive if they are pulling it off repeatedly.

Kind regards,
Joe

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2