Mon, 1 Aug 2005 10:24:08 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Lee parker <[log in to unmask]>
Parts/Attachments:
text/plain (117 lines)
Edwin

I agree with George that we do not understand black pad well enough to create an absolute test and then guarantee that that product will be free of the defect. What suppliers can do that to a some extent will minimize the likelihood is to guarantee that the product was built to the chemical suppliers process instructions. Keep in mind though this will dictate the thickness of the gold and nickel. 

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389 
  ----- Original Message ----- 
  From: Wenger, George M.<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Monday, August 01, 2005 9:07 AM
  Subject: Re: [TN] RoHs board surface recommendations.


  Edwin,

  I'm not sure platers can give a guarantee that the boards they send are Black Pad Free because all of the evaluations I've seen that were run to determine what causes Black pad didn't show any problems.  If a plater can't intentionally generate Black Pad failures then I'm not sure how they are going to provide Black Pad Free boards until they understand the root cause.

  Regards,
  George
  George M. Wenger
  Reliability / FMA Engineer
  Base Station and Subsystems Group
  Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 [log in to unmask]<mailto:[log in to unmask]>


  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]]On Behalf Of Edwin Louis
  Sent: Monday, August 01, 2005 8:38 AM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: Re: [TN] RoHs board surface recommendations.


  Ask the plater for black pad free ENIG.

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]] On Behalf Of George Milad
  Sent: Friday, July 29, 2005 7:14 AM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: Re: [TN] RoHs board surface recommendations.

  Do not discount ENIG.
  There is data available now showing that soldering to the Ni surface at the
  SAC alloy temperature conditions produces a very robust solder joint.
  There are Ni baths available now that are RoHS compliant i.e. no Cd and no
  PB.

  Best  regards

  George Milad
  [log in to unmask]<mailto:[log in to unmask]>
  National Accounts Manager  for Technology
  Uyemura International Corporation
  Technical Center
  240  Town LIne Rd
  Southington CT 06489
  (516) 901 3874 (mobile)
  (860)  793-4011 (office)
  (860) 793-4020 (fax)

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
  for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
  847-615-7100 ext.2815
  -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

  ------------------------------------------------------------------------------------------------
  This message is for the designated recipient only and may
  contain privileged, proprietary, or otherwise private information.  
  If you have received it in error, please notify the sender
  immediately and delete the original.  Any unauthorized use of
  this email is prohibited.
  ------------------------------------------------------------------------------------------------
  [mf2]

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2