TECHNET Archives

August 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 1 Aug 2005 09:07:22 -0400
Reply-To:
"Wenger, George M." <[log in to unmask]>
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Comments:
RFC822 error: <W> REPLY-TO field duplicated. Last occurrence was retained.
Parts/Attachments:
text/plain (104 lines)
Edwin,

I'm not sure platers can give a guarantee that the boards they send are Black Pad Free because all of the evaluations I've seen that were run to determine what causes Black pad didn't show any problems.  If a plater can't intentionally generate Black Pad failures then I'm not sure how they are going to provide Black Pad Free boards until they understand the root cause.

Regards,
George
George M. Wenger
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Edwin Louis
Sent: Monday, August 01, 2005 8:38 AM
To: [log in to unmask]
Subject: Re: [TN] RoHs board surface recommendations.


Ask the plater for black pad free ENIG.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of George Milad
Sent: Friday, July 29, 2005 7:14 AM
To: [log in to unmask]
Subject: Re: [TN] RoHs board surface recommendations.

Do not discount ENIG.
There is data available now showing that soldering to the Ni surface at the
SAC alloy temperature conditions produces a very robust solder joint.
There are Ni baths available now that are RoHS compliant i.e. no Cd and no
PB.

Best  regards

George Milad
[log in to unmask]
National Accounts Manager  for Technology
Uyemura International Corporation
Technical Center
240  Town LIne Rd
Southington CT 06489
(516) 901 3874 (mobile)
(860)  793-4011 (office)
(860) 793-4020 (fax)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
 
- CONFIDENTIAL-
This email and any files transmitted with it are confidential, and may also be legally privileged.  If you are not the intended recipient, you may not review, use, copy, or distribute this message. If you receive this email in error, please notify the sender immediately by reply email and then delete this email.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2