TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="ISO-8859-1"
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 12 Jul 2005 16:13:00 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mark Austin <[log in to unmask]>
Subject:
From:
Mark Austin <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (55 lines)
Try a print speed of 35 to 40mm/sec and pressure about 7Kg.

The pressure does depend on the size of the board you are printing.

From memory about 0.5Kg per Inch of PCB that is in contact with the squeege.

Mark

===== Original Message from [log in to unmask] (TechNet E-Mail Forum) at
12/07/05 14:07
>Hi guys,
>
>I have one problem here and I need your expertise to help me. Ok recently
>our fine pitch IC (20mils) has shorted/bridged after printing as we change
>from leaded to lead free solder paste. Most of the bridging at the fine
>pitch occurred in parallel to squeegee moving direction. Any suggestion or
>input is greatly appreciated.
>
>Note:
>Squeegee type: metal
>Stencil thickness: laser cut (5mils)
>Solder paste: Kester EM907
>Printer: DEK288
>Separation speed: 2mm/sec
>Printing speed: 25mm/sec
>Squeegee pressure: 8Kg
>
>
>Best Regards,
>Azman
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2