Hi guys,

I have one problem here and I need your expertise to help me. Ok recently
our fine pitch IC (20mils) has shorted/bridged after printing as we change
from leaded to lead free solder paste. Most of the bridging at the fine
pitch occurred in parallel to squeegee moving direction. Any suggestion or
input is greatly appreciated.

Note:
Squeegee type: metal
Stencil thickness: laser cut (5mils)
Solder paste: Kester EM907
Printer: DEK288
Separation speed: 2mm/sec
Printing speed: 25mm/sec
Squeegee pressure: 8Kg


Best Regards,
Azman

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2