Steve -
I would not use any of these that show this condition. DFSM is prone to
adhesion failures from lamination issues as well as surface conditions.
Adhesion issues at this stage indicate an acute problem with adhesion
and it appears from the micrographs to be from surface contamination.
This condition will likely propagate from assembly and operation of the
unit over time.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: Stephen Gregory [mailto:[log in to unmask]]
Sent: Thursday, June 02, 2005 10:51 AM
To: [log in to unmask]
Subject: [TN] Dry Film Soda Strawing...
Mornin' all ya'll...
We've got some boards in here with dry-film mask "soda strawing".
I've got pictures up on my page at: http:// www.stevezeva.homestead.com
and look at "Soda Strawing, Soda Strawing 2, 3, and 4".
These are class 3 boards and I say that if there's any evidence of soda
strawing
it's nonconforming, no matter if the soda straw is completely sealed or
even if it
doesn't reduce the conductor spacing below the minimum requirements.
If you see it on a class 3 board, it's rejectable according to the
IPC-600G
is the way I
read it...am I wrong?
BTW, I'm definately rejecting the board in the picture "Soda Strawing
4".
That picture
is over a planar transformer pattern and has the trace exposed. The
other
three pictures
are the different degrees of soda strawing that I'm seeing...is any of
it
acceptable?
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|