TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Eddie Rocha <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Eddie Rocha <[log in to unmask]>
Date:
Thu, 12 May 2005 07:33:56 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
Your callout is fine, but you can't expect 2L pricing.
Material costs for such a thick bd are going to be similar
to a 6 layer bd. and lamination costs will be included.

Thank you,
Eddie Rocha
South Bay Circuits


Hi,
This is a question to all the fab people.
My project requires a PCB that will have a finished
thickness of 4.7 mm.  I
haven't found anyone who has a standard thickness very
close, but know that
it's possible to build much thicker boards.  What is the
best way to call
out such a construction?

The other significant details are:

- 2 layers, 1/2 oz. cu
- No plated through holes
- Gold flash finish, no soldermask
- Material will be in two versions, one FR4 and one in a
hi-freq.substrate
- Boards will have an additional "cover" substrate layer
laminated over the
top, but this is not included in the 4.7 mm thickness

I hope that was clear enough.

Thank you very much for any light you can shed on this.
Richard

---------------------------------------------------
Technet Mail List provided as a service by IPC using
LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with
following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2