Hi Bev,
It sort of dependents. First there is no such thing as intermittent
micro-cracks in SJs. If they are micro-cracks, they can be present starting about 40%
into the life of the SJs, but they do not impact electrical signals,
intermittent or otherwise. If you have a full solder joint fracture, electrical signal
interruption will be intermittent, because the fracture surfaces are in at
least some slight compression and make very good 'connector surfaces.'
If you have fully fractures SJs, they will only show intermittent opens if
they are disturbed by either temperature changes or mechanical shock/vibration.
The best way to find them is to do functional tests during vibration loading.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|