Hi Bruce - what Army program is requiring the use of a Pbfree solder?
Dave Hillman
Rockwell Collins
[log in to unmask]
Bruce D Stilmack
<[log in to unmask]
M> To
Sent by: Leadfree [log in to unmask]
<[log in to unmask] cc
>
Subject
Re: [LF] Lead-Free Acceleration
01/10/2005 03:13 Factor
PM
Please respond to
"(Leadfree
Electronics
Assembly Forum)"
<[log in to unmask]
>; Please respond
to
[log in to unmask]
Remember, this is not just Europe. We currently have requirements to use
LF on one of the Army's new vehicle programs.
Bruce Stilmack
GDLS-TO Manufacturing Engineer
(850) 574-4773
[log in to unmask]
Werner Engelmaier
<[log in to unmask] To: [log in to unmask]
OM> cc:
Sent by: Leadfree Subject: Re: [LF] Lead-Free
Acceleration Factor
<[log in to unmask]
>
01/10/2005 03:46
PM
Please respond to
"(Leadfree
Electronics
Assembly Forum)";
Please respond to
Engelmaier
Hi Pascal,
At this point I would not put LF-solders into anything other than consumer
products. If you have to depend on reliability, and worse, have severe use
conditions there are no guarantees.
I would suggest building an A300 with LF-solders in the electronics, and
fly
all the responsible [should be irresponsible] Brussel bureaucrats on it
exclusively.
Werner
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-------------------------------------------------------------------------------
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-------------------------------------------------------------------------------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|