Subject: | |
From: | |
Reply To: | (Leadfree Electronics Assembly Forum) |
Date: | Thu, 6 Jan 2005 09:29:31 -0700 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
We are seeing components with this finish. There is data to support the
acceptability of a final lead finish containing up to 3% Bismuth.
Dewey
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of Genny Gibbard
Sent: Thursday, January 06, 2005 9:15 AM
To: [log in to unmask]
Subject: [LF] The use of Bismuth
So I am curious, what are people thinking about the use of bismuth in lead
free termination finishes. I am not talking about solder containing Bi.
The only supplier I have come across so far specifically mentioning they use
Bi is NEC. They have a doc on their website, called "Japan's best kept
secret" http://www.cel.com/pdf/marcomnews/japan_best.pdf that claims
that SnBi is recommended by JEITA, as opposed to the recommendation of JEDEC
for Matte Sn. They make it sound as if a lot of companies are using this
plating, but I haven't come across any other components so far that use it.
The main concern I have is that I keep getting the impression that the next
metal that the EU will be gunning for eliminating is Bi, so it doesn't sound
like a smart direction to go.
Thoughts?
Genny Gibbard (mailto:[log in to unmask])
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|