Bill,
Could conformal coating stop the whiskers from forming
after assembly?
No, but it can slow it down some.
David A. Douthit
Manager
LoCan LLC
Brooks,Bill wrote:
>I showed the tin whisker nightmare photo's to an RF engineer I know here and
>she said that they had similar problems years ago in the Space applications
>field and the solved it by coating the surface with 'Q-Dope' a
>polystyrene/tolulene
>
>Q-Dope
>http://www.takefiveaudio.com/gc_q_dope.htm
>
>Material/Safety specs
>http://www.chess.cornell.edu/Safety/MSDS/polystyrene_Q_Dope.htm
>
>TIN Whisker Pictures
>
>http://nepp.nasa.gov/whisker/photos/waveguide/index.html
>
>
>Maybe the solution to TIN plating issues is some sort of coating or barrier
>to prevent whiskers? Could conformal coating stop the whiskers from forming
>after assembly?
>
>(Makes you wonder why we are even caving in to the pressure to change from
>tin/lead solder....)
>
>
>
>Bill Brooks - KG6VVP
>PCB Design Engineer , C.I.D.+, C.I.I.
>Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
>e-mail:[log in to unmask]
>http://www.dtwc.com
>http://pcbwizards.com
>
>-------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|