Steve,
Solder oxidizes more readily then tin but if there is no contact then as
they say "no harm no foul".
Is this electroplated, electroless, or immersion plated tin over nickel
(how thick is the tin)?
I would be more concerned with whiskers!
David A. Douthit
Manager
LoCan LLC
-------------------------------
Steve Gregory wrote:
>Yes David, they are tin plated. See the following datasheet:
>
>_http://www.samtec.com/ftppub/pdf/PCT2.PDF_
>(http://www.samtec.com/ftppub/pdf/PCT2.PDF)
>
>I have a couple of questions:
>
>1. Is 63% tin and 37% lead so dissimilar that it would create conditions for
>dissimilar metal corrosion?
>
>2. If the solder didn't flow up into the wiping area of the contact (from my
>observations, it didn't) should we still replace the connector?
>
>Sorry to be beating a dead-horse to death, but I want truely want to
>understand why the rework that we did was so bad...I want to learn from this
>experience.
>
>-Steve Gregory-
>
>Steve,
>
>The only reason I can think of is that the mating pins are also tin
>plated and a layer of solder would create dissimilar metal corrosion.
>
>David A. Douthit
>Manager
>LoCan LLC
>
>
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|