Hi folks
Not sure how else to avoid the commercial but take a look at our web site
please? It is at the bottom of this message. I am dismayed that we didn't
register on the search so will try to do something about that.
As to the question regarding trailing wires, you need to attach a
thermocouple to various points on the assembly - using aluminium tape to
secure them! - the thermocouple wire is then attached to a measurement
device (the profiler). You might want to mount the profiler piggy-back to
the assembly but be careful that this does not compromise your results.
I hope this helps and I don't get flamed for the commercial....
--
Regards Graham Naisbitt
[log in to unmask]
Concoat Limited - Engineering Reliability in Electronics
A British Manufacturer
NEW WEB SITE: www.concoat.co.uk :NEW WEB SITE
Golf Quote of the week: The Royal Hong Kong Golf Club caddies hit the nail
on the head; their term for golf: "Hittee ball, say damn."
Cell: 079 6858 2121
Office: +44 (0)1252 813706
> From: "Black, Paul" <[log in to unmask]>
> Reply-To: TechNet E-Mail Forum <[log in to unmask]>, "Black, Paul"
> <[log in to unmask]>
> Date: Tue, 26 Oct 2004 10:21:34 -0400
> To: <[log in to unmask]>
> Subject: Re: [TN] Profiler
>
> Tom,
>
> I'm going through the same process right now. I have the same two names as
> you, plus ECD, which makes the Super MOLE. You can try them @
> http://www.ecd.com/
>
>
> Paul Black
> Manufacturing Engineer
> Kronos
> E-mail: [log in to unmask]
> Voice: (978) 947-1520
> Fax: (978) 244-0568
>
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Tom Parkinson
> Sent: Tuesday, October 26, 2004 10:02 AM
> To: [log in to unmask]
> Subject: [TN] Profiler
>
>
> Can you suggest various SMT profiler's available?
>
> I did a Google search, but the results were very poor. I am aware of the
> KIC system, and Datapaq.
>
> We're looking for a profiler that can go through the oven with the PCB
> assembly, not one that strings out the probe wires (they always get stuck in
> the conveyor...) Any suggestions would be appreciate.
>
> You can contact me off net if your worried about it sounding like an
> advertisement. Thanks
>
> Tom Parkinson - Quality System Manager - CIT
> WinTronics, Inc.
> Ph: 724-981-5770 Ext. 235
> Fax: 724-981-1772
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|