It would be interesting to know how you are measuring this phenomena. A
decrease in insulation resistance could be caused by the same things that result
in dendrites after humidity and bias. If you have visual dendrites without any
bias, we need to know more and see photos.
Susan Mansilla
Robisan Lab
---------------------------------------------------