TECHNET Archives

September 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Date:
Wed, 29 Sep 2004 10:19:00 -0700
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ted Kong <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (261 lines)
        Hi Ted:
        What was your particular land design ( shape of the lands ) for the 0402s that work well for you?
        Regards,
        Ramon

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ted Kong
Sent: Wednesday, September 29, 2004 12:17 PM
To: [log in to unmask]
Subject: Re: [TN] ENIG vs. HASL plating with 0.5 mm pitch QFN components


Hi, Joe,

one of our design has 0402 and QFNs on the board and
we use HASL with 4 mils stencils.  Our factory did not
report any issue.  One thing to keep in mind is that
you must have a good pad design for 0402 land pattern
to prevent insufficient solder or tombstoning.


Ted
--- "Wenger, George M." <[log in to unmask]>
wrote:

> Paul,
>
> I didn't make any comment about planarity or
> indicate that HASL couldn't be controlled and used
> for 0.5mm pitch because there are lots of companies
> using HASL for 0.5mm pitch.  The reason I wouldn't
> recommend HASL is because of the pending RoHS/WEEE
> directives.
>
> Regards,
> George
>
> George M. Wenger (908)-546-4531
> Reliability / FMA Engineer
> Base Station and Subsystems Group
> Andrew Corporation,  40 Technology Drive, Warren, NJ
> 07059
> [log in to unmask]
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of
> Paul Edwards
> Sent: Monday, September 27, 2004 4:34 PM
> To: [log in to unmask]
> Subject: Re: [TN] ENIG vs. HASL plating with 0.5 mm
> pitch QFN components
>
>
> Joe,
>
> I disagree with Paul and George...
>
> The planarity issue with HASL on .5mm pitch parts is
> over blown.
> A good PCB fabricator can control HASL variations.
>
> HASL increases the volume of solder in the lap joint
> and increases and
> lowers the joint's bulk interface intermetallics.
>
>
> Paul
>
> Paul Edwards
> Process Engineering
> [log in to unmask]
> Tel: 408-433-4700
> FAX: 408-433-9988
> Surface Art Engineering
> 81Bonaventura Dr.
> San Jose, CA 95134
> DUNS: 944740570
> CAGE/NCAGE: 1XZ48
>
> -----Original Message-----
> From: Black, Paul [mailto:[log in to unmask]]
> Sent: Monday, September 27, 2004 11:40 AM
> To: [log in to unmask]
> Subject: Re: [TN] ENIG vs. HASL plating with 0.5 mm
> pitch QFN components
>
> Joe,
>
> I would agree with George on both counts. In any
> case, I wouldn't choose
> HASL. It doesn't deposit evenly. In the case of your
> fine pitch and small
> components, you could end up with reliability
> issues.
>
> Thank you,
> Paul Black
> Manufacturing Engineer
> Kronos
> E-mail: [log in to unmask]
> Voice: (978) 947-1520
> Fax: (978) 244-0568
> www.kronos.com
> Improving the Performance of People and Business(tm)
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of
> Wenger, George M.
> Sent: Monday, September 27, 2004 1:21 PM
> To: [log in to unmask]
> Subject: Re: [TN] ENIG vs. HASL plating with 0.5 mm
> pitch QFN components
>
>
> Joe,
>
> Were you asked to recommend the type of pwb plating
> that is best for your
> simple board or were you only given two choices to
> pick from?  If I had to
> pick from the two choices I'd pick ENIG.  If I had
> to make a recommendation
> I wouldn't recommend either.  My preference would be
> immersion silver.
>
> Regards,
> George
>
> George M. Wenger (908)-546-4531
> Reliability / FMA Engineer
> Base Station and Subsystems Group
> Andrew Corporation,  40 Technology Drive, Warren, NJ
> 07059
> [log in to unmask]
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of
> Macko, Joe @ IEC
> Sent: Monday, September 27, 2004 1:08 PM
> To: [log in to unmask]
> Subject: [TN] ENIG vs. HASL plating with 0.5 mm
> pitch QFN components
>
>
> Fellow techs,
>
> I have been asked to recommend the type of pwb
> plating that is best for a
> simple board with only a few components.  The finest
> pitch component is a
> QFN, 64 pads, 0.5 mm pitch.  There are some 0402
> resistors and capacitors as
> well.
>
> My 2 choices are HASL or ENIG.  Would someone please
> comment on which is
> best for 0402  and 0.5 mm QFN type components.
>
> Thanks in advance.
> joe
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach
> Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
>
-----------------------------------------------------
>
>
----------------------------------------------------------------------------
> --------------------
> This message is for the designated recipient only
> and may
> contain privileged, proprietary, or otherwise
> private information.
> If you have received it in error, please notify the
> sender
> immediately and delete the original.  Any
> unauthorized use of
> this email is prohibited.
>
----------------------------------------------------------------------------
> --------------------
> [mf2]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach
> Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
>
-----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV
=== message truncated ===




_______________________________
Do you Yahoo!?
Declare Yourself - Register online to vote today!
http://vote.yahoo.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2