TECHNET Archives

September 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Date:
Wed, 29 Sep 2004 08:03:38 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (143 lines)
        Hi A.N. Prasad
        It is time for a DOE.  Find out if it is the same LEDs failing. Assemble one board by hand and see if you have the same problem, it could be that LEDs are not taking the reflow temp.  Retouch the joints of the LEDs that fail and connecting circuitry, include input voltage and current limiting resistor, see if the LEDs come on after doing so.
        Regards,
        Ramon

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Wenger, George M.
Sent: Wednesday, September 29, 2004 6:02 AM
To: [log in to unmask]
Subject: Re: [TN] Reliability issue in 0402 soldering


A.N.,

Fabrizio is correct that the PCB finish influences the soldering.  However, poor soldering can influence the operation of the LEDs.  Since all of the LEDs work immediately after assembly and a few stop working sometime later, it sounds like you may have a few resistors that are not soldered well.  I would suggested a detailed inspection of the resistors especially those associated with the LEDs that are not working to see if you have good solder joints.

Regards,
George
George M. Wenger, Andrew Corporation
Reliability / FMA Engineer
Base Station & Subsystems Group
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [log in to unmask]
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fabrizio Ramari (framari)
Sent: Wednesday, September 29, 2004 5:47 AM
To: [log in to unmask]
Subject: Re: [TN] Reliability issue in 0402 soldering

The PCB finishing influence the soldering not the function . 
Fabrizio
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Janoch Jirí, Ing.
Sent: Wednesday, September 29, 2004 11:34 AM
To: [log in to unmask]
Subject: Re: [TN] Reliability issue in 0402 soldering

Hi,
we use PCB ENIG surface for tiny components but I would say that PCB tin
surface does not influence on LED function.

J.Janoch, Des. Dpt.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Prasad AN
Sent: Wednesday, September 29, 2004 10:14 AM
To: [log in to unmask]
Subject: [TN] Reliability issue in 0402 soldering

Hi all

We are assembling around 750 # of 0402 size LEDs in small PCB of size
65mm X
65mm.

The problem we are having after reflow, when PCB is tested all the LEDs
are
glowing.

But after some time the problem starts with 3-4 LEDs not glowing.

The PCB surface is of  Tin plating.

Let me know is the PCB surface is suitable for this type of board. If
not
what type of surface is recommended for PCB with only 0402 LEDs.


Thanks with Warm regards

A.N.Prasad




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2