These are old callouts that date back to pre-1977 changes to the MIL
spec 13949.
They refer to "hot-strength retention" epoxy glass laminates for
double-sided. GB is non-FR. GH is FR. See slash sheets 3 and 5 (?)
for the old MIL-P-13949.
In IPC-4101A, the spec sheets that apply to these are GB => 4101/22 and
GH => 4101/23.
Today, most laminators will offer you their 170C FR4, which are covered
by 4101/24, but some laminators have dual qualification to the /23 also.
I don't think any non-FR epoxy resin is used today. People just
substitute the FR versions.
Jim Paulus
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin D Asbell
Sent: Wednesday, September 15, 2004 11:21 AM
To: [log in to unmask]
Subject: [TN] Laminate question
Got a spec with the following information;
Type FL-GH or FL-GB,
Does anyone know what these refer to???
Thanks
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
Franklin
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|