TECHNET Archives

September 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 15 Sep 2004 14:14:48 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Black, Paul" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Black, Paul" <[log in to unmask]>
Parts/Attachments:
text/plain (119 lines)
Hi Everyone,

I have a question regarding this issue; my limited experience with plugging is that it doesn't sit flush at the top of the via but is somewhat raised. Wouldn't this cause problems printing during solder deposition?

Thank you, 
Paul Black 
Manufacturing Engineer 
Kronos 
E-mail: [log in to unmask] 
Voice: (978) 947-1520 
Fax: (978) 244-0568 
www.kronos.com 
Improving the Performance of People and Business(tm) 



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Charles Caswell
Sent: Wednesday, September 15, 2004 10:59 AM
To: [log in to unmask]
Subject: Re: [TN] Question about via masking on BGA pattern...


I can agree to this. I suggested covering both sides just because most of our
customers question uncovered via's. Not sure why, especially those with
specific notes on drawing to leave via's unplugged and not masked.

-----Original Message-----
From: Jeffrey Bush [mailto:[log in to unmask]] 
Sent: Wednesday, September 15, 2004 7:56 AM
To: [log in to unmask]
Subject: Re: [TN] Question about via masking on BGA pattern...

I would recommmend the opposite of this - plug from the BGA side and
leave the bottom open for testing.



Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com	



-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]] 
Sent: Wednesday, September 15, 2004 8:44 AM
To: [log in to unmask]
Subject: [TN] Question about via masking on BGA pattern...


Mornin' All!

I have a question about solder masking via's in a BGA pattern, and want
to see if I'm thinking correctly about this.

I think it's a bad idea to leave the via's free from solder mask on the
topside of the board beneath the BGA, and tent the bottomside via's. To
me, you're just asking for trouble down the road because you'll trap
flux residue and all kinds of stuff in the via's that won't be able to
be cleaned out well. This is a 676 ball 1.0mm pitch BGA pattern. Am I
wrong about this?

Thanks!

-Steve Gregory-

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2