TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Reeves, Tim R." <[log in to unmask]>
Date:
Mon, 23 Aug 2004 12:29:26 -0400
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Colin Weber <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Reeves, Tim R." <[log in to unmask]>
Parts/Attachments:
text/plain (86 lines)
Here's the link I believe you are referring to:

http://www.datacircuits.com/docs/Full%20Material%20Sheet.pdf


I noticed when I looked at my Rogers book that 4003C is not UL 94V-0, while
4350B is. So it is the 4003C that is working for you, right?
I also notice that 4003C has a little bit lower Dk and a lower tan delta
than the 4350B. Perhaps it's the tan delta that's key and a PTFE-based
material like Taconic RF-35 (which does have UL 94V-0 rating) will work for
you. (It's not on the list at the URL above)
Also, the Arlon 25N that Jeffrey suggested is not 94V-0 rated, but 25FR is.
Unfortunately, the tan delta of the 25FR is higher (like that of 4350B).


Tim Reeves
Materials/Lamination Engineer
Tyco Printed Circuit Group - Dallas Division
(800) 783-9223   ext. 1120


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Colin Weber
Sent: Sunday, August 22, 2004 3:53 PM
Subject: Re: Search for HF Laminate Material


Hi Phil,

I tried that link at the time and it didn't work so I trashed it. Maybe
there was
a problem with our Intranet at the time. Do you still have that link?

Tim and Ingemar,

We are not using embedded/buried capacitors. The capacitance we wish to
achieve is
on external layers using copper pads. We succeed with the rogers non-UL
material.
Now we need to replicate the results with a UL material. We are looking to
create
a capacitance of 0.25pF and these are used in sampling 3.5kV of RF. We do
not
know precisely what didn't work with the UL Rogers material and why the
non-UL
did work. At this stage we are just trying different materials and looking
at end results for our application, of which I am unable to describe in
detail.


Colin


At 01:44 AM 8/21/2004, you wrote:
>hi,
>
>a couple days ago a url was provided that presented a very extensive table
of
>properties for several vendors laminate products.  did  you check there?
>
>phil

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2