Meet or exceed which numbers, and which way?
Are you talking about embedded/buried capacitors? If so there are materials
especially designed for this, like ZBC (from various laminators), DuPont
Interra, etc.
Usually lower dielectric constant would be thought of as better material,
except when you want capacitance; then higher Dk is better, and Rogers 4003
or 4350 both have fairly low Dk. Good for RF, not so good for BC.
Tim Reeves
Materials/Lamination Engineer
Tyco Printed Circuit Group - Dallas Division
(800) 783-9223 ext. 1120
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Colin Weber
Sent: Thursday, August 19, 2004 9:37 PM
Subject: Search for HF Laminate Material
Hi Folks,
Does anybody know of a material which can meet or exceed the
following specifications for a Rogers RO4003C, which has UL
approval (94V-0)?
Dielectric Constant 3.38 +-0.05
Dissipation Factor tan 0.0027/0.0021
Temperature Coefficient +40 ppm/deg. C
Coefficient of Thermal Expansion x=11, Y=14, Z=46 ppm/deg. C
water absorption 0.04%
FR4 standard Processing
The application is for making capacitors out of PCB material.
The Rogers RO4350B UL material did not perform as well as the
RO4003C.
Regards,
Colin Weber
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|