TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Crawford <[log in to unmask]>
Date:
Fri, 20 Aug 2004 14:37:25 +1000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Colin Weber <[log in to unmask]>
Subject:
From:
Colin Weber <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"; format=flowed
Parts/Attachments:
text/plain (34 lines)
Hi Folks,

Does anybody know of a material which can meet or exceed the
following specifications for a Rogers RO4003C, which has UL
approval (94V-0)?

Dielectric Constant 3.38 +-0.05
Dissipation Factor tan 0.0027/0.0021
Temperature Coefficient +40 ppm/deg. C
Coefficient of Thermal Expansion x=11, Y=14, Z=46 ppm/deg. C
water absorption 0.04%

FR4 standard Processing

The application is for making capacitors out of PCB material.
The Rogers RO4350B UL material did not perform as well as the
RO4003C.



Regards,

Colin Weber

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2