There's also a kit availiable from www.LeadCheck.com. The kit consists
of swabs that have a lead reactive dye inside.
Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> [log in to unmask] 08/18/04 03:18PM >>>
You can find a reasonably sensitive, inexpensive and quick spot test
kit
for lead at the following site:
http://www.leadinspector.com/
I'm not too sure that I will use it for more than a quick
verification.
If the part fails or is borderline I'll probably go to a more
sensitive
analytical method.
Rich K / KEDS
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bloomquist, Ken
Sent: Wednesday, August 18, 2004 8:07 AM
To: [log in to unmask]
Subject: Re: [TN] Tests For Component Finish
Ingemar/Joe,
I don't know about your part of the world but our labs are expensive.
If
we were to test everything that came in we'd go broke!
What really needs to happen is for the component industry to adopt a
universal code that will identify the lead finish. [L] for lead, [T]
for
tin, [G] for gold, etc. or something like that. They would add this to
the end of their part number and it would resolve all questions.
My 2C worth,
KennyB
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Tuesday, August 17, 2004 11:52 PM
To: [log in to unmask]
Subject: Re: [TN] Tests For Component Finish
Joe,
we are thinking likewise. Best of all is of course to have good and
reliable suppliers, and make clear specs that tell them what you want.
Unfortunately, that's dreaming about component paradise. So, we need
to
be realistic and check to be sure. In my opinion there is one
reliable
and good and fast way to find out about the finish:
1. cross section a sample and have a look in a metallurgical
microscope.
2. if you are still uncertain, send the samples to someone with an EDS
why buy an EDS? There are plenty of analysis labs around.
Ingemar Hernefjord
Ericsson Microwave Systems
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|