TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Date:
Wed, 18 Aug 2004 15:43:09 +0200
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Bloomquist, Ken" <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Parts/Attachments:
text/plain (68 lines)
Right! And that is a MEGAtopic at our company. Imagine when we get a million pcs delivery, and the finish is wrong. Except for bad words and stomachs, it costs a fortune to correct. And..sometimes, you need look under the finish too. E.g. we had been mounting a lot and had sent products to various customers, when we realized that the shiny and easily soldered terminals hid a disastrous kind of failure: the barrier nickel didn't wet enough on the terminal bulk metal. So, the hermetic packages turned into leakers rather soon. And the manufacturer of those simple components did not even understand our analysis report.

So, 'just in time' is sometimes 'maybe in time', which is not acceptable.

Ingemar


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bloomquist, Ken
Sent: den 18 augusti 2004 15:07
To: [log in to unmask]
Subject: Re: [TN] Tests For Component Finish


Ingemar/Joe,

I don't know about your part of the world but our labs are expensive. If we were to test everything that came in we'd go broke!

What really needs to happen is for the component industry to adopt a universal code that will identify the lead finish. [L] for lead, [T] for tin, [G] for gold, etc. or something like that. They would add this to the end of their part number and it would resolve all questions.

My 2C worth,

KennyB

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Tuesday, August 17, 2004 11:52 PM
To: [log in to unmask]
Subject: Re: [TN] Tests For Component Finish


Joe,
we are thinking likewise. Best of all is of course to have good and
reliable suppliers, and make clear specs that tell them what you want.
Unfortunately, that's dreaming about component paradise.
 So, we need to be realistic and check
 to be sure. In my opinion there is one reliable and good and fast
 way to find out about the finish:

1. cross section a sample and have a look in a metallurgical microscope.
2. if you are still uncertain, send the samples to someone with an EDS

why buy an EDS? There are plenty of analysis labs around.

Ingemar Hernefjord
Ericsson Microwave Systems

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2