TECHNET Archives

July 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Tom Parkinson <[log in to unmask]>
Date:
Thu, 8 Jul 2004 11:54:36 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Reuven ROKAH <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Parts/Attachments:
text/plain (79 lines)
Siemens Siplace machines had this option in the past but not longer because
of time consumption take for the testing.

You can try to find such old versione  (Siplac S15 / F3)  in the used
machine market.

Best  Regards

Reuven  ROKAH




                      Tom Parkinson
                      <tomp@WINTRONICS         To:      [log in to unmask]
                      INC.COM>                 cc:
                      Sent by: TechNet         Subject: [TN] Mydata Info
                      <[log in to unmask]
                      >


                      07/07/2004 20:43
                      Please respond
                      to "TechNet
                      E-Mail Forum.";
                      Please respond
                      to Tom Parkinson





One of our customers has said their other CM uses a Mydata SMT pick and
place system that has the 'on-the-fly' testing. From what our customer
says,
this testing will catch all marginal passive parts, including any SMT caps
that may have very small cracks.



Anyone have experience with this 'on-the-fly' testing option?



Tom Parkinson - Quality System Manager - CIT

WinTronics, Inc.

Ph: 724-981-5770 Ext. 235

Fax: 724-981-1772




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2