Because there is no reasonable costing high temp solder to replace the
existing high temp solder it has been exempt from the lead free
requirements. I will look through my archive documents about this
subject but I am pretty sure this has been approved and is part of the new
lead free requirements.
Steve Gregory
<[log in to unmask] To: [log in to unmask]
M> cc:
Sent by: TechNet Subject: [TN] Lead Free BGA's...
<[log in to unmask]>
05/28/04 10:30 PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
SteveZeva
Hi ya'll!!!
I know most everyone is out for the Memorial day holiday, so this will be
something that
everyone can look at on Tuesday...
My question is; what are the spheres going to be made of for "Lead-Free"
BGA's? What about the BGA's (ceramic ones usually) that have "High-temp"
balls?
The high-temp balls are mostly lead, right?
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
STATEMENT OF CONFIDENTIALITY:
If you have received this e-mail in error, please immediately notify the
sender by e-mail at the address shown. This e-mail and any attachments may
contain confidential information. This information is intended only for the
use of the individual(s) or entity to whom it is intended even ifaddressed
incorrectly. Please delete it from your files if you are not the intended
recipient. Thank you for your compliance.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|