Dear colleagues,
PCBs that include some nets have one end point carbon buttons and other end
point normal pad, are covered with OSP the normal pads turns brown by time.
Can you explain What is its reason?
Best Regards,
Mustafa YÜCEL
Product Quality Engineer
BASKI DEVRE SAN. ve TIC. LTD. STI.
Ceyhan Sk. No:10 81490 Pendik-Istanbul-Turkey
Tel: 00 90 216 3901036 (4 Hat/Line)
00 90 216 4836560 (4 Hat/Line)
Fax: 00 90 216 3544941
00 90 216 4913269
Internet: www.baskidevre.com.tr
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------