Sender: |
|
Subject: |
|
From: |
|
Date: |
Wed, 7 Apr 2004 08:52:15 -0500 |
X-To: |
|
Reply-To: |
|
Parts/Attachments: |
|
|
I have seen BGA intermittents caused by excessively large voids within the
BGA balls (verify with X-ray) especially if via in pad was used. Also black
pad is a possibility if the finish was ENIG.
Regards,
Bruce Misner
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, April 07, 2004 9:34 AM
To: [log in to unmask]
Subject: Re: [TN] BGA soldering issue
Hi SJ!
I've heard of this problem more than just a few times. Former TechNetter
Earl
Moon ran across this problem and solved it easily.
You can go to: http://www.stevezeva.homestead.com and look at "Creative
Engineering" at the top left-hand picture there. What? You don't want to fix
the
problem like Earl did? Why not?
Just kidding...Earl did what he had to do so the board would play. I believe
in his case it was more part related than any manufacturing issue.
I've had an intermittent connection with a BGA once. It was a VERY expensive
560-ball Xilinx device, that I really didn't want to have to remove and
replace because of it's price. The part had eutectic balls.
Test said the part would play when pressed on. So I figured I had nothing to
lose by fluxing the part liberally beneath it, and then taking it over to my
rework station to reflow the BGA and hope that maybe the intermittent
connection would heal itself.
The soldering gods were with me that day and it worked. The board passed the
initial test after rework, as well as subsequent tests after thermal
cycling.
Some days you're just lucky I guess...
-Steve Gregory-
> Dear Technetters,
>
> We encountered BGA chip having intermitten contact issue in our
prototypes.
> When we pressed hard on the BGA chip, the prototype worked ok. We need
advice
>
> on how to tackle this issue from prototype building's point of view. What
> measures should be taken to make sure "no contact issue" during prototype
> building.
>
> Your advice is very much appreciated. Thanks in advance.
>
> Best regards,
> SJ Liew
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|