TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Misner, Bruce" <[log in to unmask]>
Date:
Wed, 7 Apr 2004 10:01:06 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (123 lines)
Yes I agree - also look at the geometry of the BGA pads - do they make
the device specs and watch for "hot-dog" shaped ball to via runs, these
can starve paste from the standoff and create opens, usually on finer
pitch arrays.


Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com	



-----Original Message-----
From: Misner, Bruce [mailto:[log in to unmask]] 
Sent: Wednesday, April 07, 2004 9:52 AM
To: [log in to unmask]
Subject: Re: [TN] BGA soldering issue


I have seen BGA intermittents caused by excessively large voids within
the BGA balls (verify with X-ray) especially if via in pad was used.
Also black pad is a possibility if the finish was ENIG.

Regards,
Bruce Misner

-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, April 07, 2004 9:34 AM
To: [log in to unmask]
Subject: Re: [TN] BGA soldering issue


Hi SJ!

I've heard of this problem more than just a few times. Former TechNetter
Earl Moon ran across this problem and solved it easily.

You can go to: http://www.stevezeva.homestead.com and look at "Creative
Engineering" at the top left-hand picture there. What? You don't want to
fix the problem like Earl did? Why not?

Just kidding...Earl did what he had to do so the board would play. I
believe in his case it was more part related than any manufacturing
issue.

I've had an intermittent connection with a BGA once. It was a VERY
expensive 560-ball Xilinx device, that I really didn't want to have to
remove and replace because of it's price. The part had eutectic balls.

Test said the part would play when pressed on. So I figured I had
nothing to lose by fluxing the part liberally beneath it, and then
taking it over to my rework station to reflow the BGA and hope that
maybe the intermittent connection would heal itself. The soldering gods
were with me that day and it worked. The board passed the initial test
after rework, as well as subsequent tests after thermal cycling.

Some days you're just lucky I guess...

-Steve Gregory-


> Dear Technetters,
>
> We encountered BGA chip having intermitten contact issue in our
prototypes.
> When we pressed hard on the BGA chip, the prototype worked ok. We need
advice
>
> on how to tackle this issue from prototype building's point of view. 
> What measures should be taken to make sure "no contact issue" during 
> prototype building.
>
> Your advice is very much appreciated. Thanks in advance.
>
> Best regards,
> SJ Liew
>


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2